New Hardening Process for our receivers
Just an FYI.... we are in the process of running out our first batch of receivers with the FULL SALTBATH HARDENING process. We will provide more details as our processes become finalized, but know that we will soon have our top-selling pre-drilled AK-47 receiver in a large quantity in stock with a Rockwell hardness from 38-42 on the C scale across the entire receiver.
This is a big step for us as we roll out large quantities. We are catering to the large-scale manufacturers now and with them come huge quantities. It just doesn't make sense to do what we were doing anymore.
Regardless, there will soon be a sale to clear out the old stock of the spot hardened receivers. Stayed tuned for a discount code to be announced in the near future!
This is a big step for us as we roll out large quantities. We are catering to the large-scale manufacturers now and with them come huge quantities. It just doesn't make sense to do what we were doing anymore.
Regardless, there will soon be a sale to clear out the old stock of the spot hardened receivers. Stayed tuned for a discount code to be announced in the near future!
LIKE us on Facebook! http://facebook.com/southernarmament
- SouthernArmament
- Posts: 33
- Joined: Sat May 05, 2012 12:13 pm
- Location: Louisville, KY
- Has liked: 0
- Been liked: 0
- Contact:
Re: New Hardening Process for our receivers
well, we aren't doing the process, we are subbing it out to the pros! That kind of equipment is large and hot! Something we don't want around but we'll happily pay this reputable company to do it for us!
We are sending quantities of at least 150 pcs per batch....
We are sending quantities of at least 150 pcs per batch....
LIKE us on Facebook! http://facebook.com/southernarmament
-
- KAC Member
- Posts: 6387
- Joined: Sat Mar 03, 2012 8:48 pm
- Location: Metro Louisville
- Has liked: 3 times
- Been liked: 15 times
- Contact:
Re: New Hardening Process for our receivers
When I work in toolmaking full time , that's what the plastic plant I worked for did.
I was in charge of heat treating and we would send out two/three parts a month.
Else a bucket of oil, furnace , and a torch is what we used.
I was in charge of heat treating and we would send out two/three parts a month.
Else a bucket of oil, furnace , and a torch is what we used.
- son of liberty
- KAC Member
- Posts: 1759
- Joined: Sat Mar 03, 2012 9:22 pm
- Location: Carrollton
- Has liked: 0
- Been liked: 0
Re: New Hardening Process for our receivers
I run salt pots, for receivers I could see salt pots doing well for controlling decarb and warping, but beyond that you are going to an extreme , im sure your customers will never really understand the extremes your going to in order to provide the very best product.
- SouthernArmament
- Posts: 33
- Joined: Sat May 05, 2012 12:13 pm
- Location: Louisville, KY
- Has liked: 0
- Been liked: 0
- Contact:
Re: New Hardening Process for our receivers
That's OK... we just want them to be the best that we can provide.
LIKE us on Facebook! http://facebook.com/southernarmament